Nanoindentation/scratching at finite temperatures: Insights from atomistic-based modeling

TitleNanoindentation/scratching at finite temperatures: Insights from atomistic-based modeling
Publication TypeJournal Article
Year of Publication2018
AuthorsChavoshi SZare, Xu S
JournalProgress in Materials Science
DOI10.1016/j.pmatsci.2018.09.002
Grant: 
CSC, MRL (new) (DMR-1720256), MRI (CNS-1725797)